Conductive TPR Pellets DGK-TPR DD6-9A
Soft conductive TPR with 10^6-10^9 ohm/sq resistance and 70 hardness
Conductive 10^6-10^9 ohm/sq; hardness 70; good elasticity.
Conductive TPR compound DGK-TPR DD6-9A with 10^6-10^9 ohm/sq resistance and 70 hardness for sealing strips, flexible ESD parts, electronic sleeves, soft conductive components and molded elastomer parts. DEYU supports custom formulas, sample validation, bulk purchase and wholesale procurement.
Important parameters
- Base resin
- TPR
- Model
- DGK-TPR DD6-9A
- Color
- Custom color matching supported
- Processing
- Injection molding / extrusion. Injection molding, extrusion or other processes according to the formula.
- Key performance
- Conductive 10^6-10^9 ohm/sq; hardness 70; good elasticity.
- Status
- Pellet compound
FAQ
Can this material be color matched?
Yes. DEYU can match black, natural, white or custom colors according to the base resin, filler system and target appearance.
Can the resistance or ESD level be customized?
Yes. Resistance range, stiffness and processing balance can be adjusted according to wall thickness, part design and grounding requirements.
Can international orders receive certification documents?
Yes. DEYU can provide material data sheets and common export documents, and can coordinate RoHS, REACH, UL-related or other third-party testing according to the order requirement.
How can I get a sample of DGK-TPR DD6-9A or a similar material?
Submit the target resin, color, process and performance range. DEYU will suggest a sample grade or prepare a trial formula for sample validation. Request sample
Application areas
| Application area | Typical parts |
|---|---|
| Application area 1 | ESD trays |
| Application area 2 | sensor housings |
| Application area 3 | medical device accessories |
| Application area 4 | conductive textile parts |
| Application area 5 | shielding covers |
| Application area 6 | low-resistance molded clips |
Reference quote
- Minimum price
- USD 4.1/kg
- Maximum price
- USD 10.3/kg
- Delivery
- Tax-included reference price; freight is not included.
- Stock
- Standard stock reference: 1000 kg. Special color, performance or certification requirements require custom production.
Final quotation depends on the specific formula, color, order volume and testing requirements.
Data sheet
Physical Property Data Sheet
| Name | TPR composite | Specification | DGK-TPR DD6-9A |
|---|---|---|---|
| Material properties | General-purpose, conductive, anti-static | Color | Black |
| Use | Wireless antenna insulating sleeves; dust covers | Sample state | Pellets |
| Processing method | Injection molding | - | / |
| Item | Condition | Method | Data | Unit |
|---|---|---|---|---|
| Mechanical Properties | ||||
| Tensile strength | / | ASTM D-412 | 4.6 | MPa |
| Elongation at break | / | ASTM D-412 | 220 | % |
| Surface resistivity | / | / | 10^6-10^9 | ohm/sq |
| Others | ||||
| Density | 23℃ | ASTM D-792 | 1.01 | g/cm3 |
| Embrittlement temperature | / | GB 1682 | -30 ± 3 | ℃ |
| Hardness | / | ASTM D-2240 | 70 | / |
| Flammability | / | UL94 | HB | / |
Contact
Focused on modified plastic R&D and production
We provide professional customization services. If you have material questions, selection difficulties or performance requirements, contact us through any method on the right.
- Email: market@deyuplastics.com
- WeChat: mkx13905842100
- WhatsApp: +86 13905842100+86 15325909695
- Telegram: @deyuplast1