Halogen-Free Flame Retardant PP Pellets DGK-PP WPP-V0

Halogen-free polypropylene reaching V-0 at 1.6 mm for flame-retardant molding

Halogen-free V-0 flame retardant; 1.6 mm can be tested to V-0; glow wire can be customized.

Halogen-free flame retardant PP compound DGK-PP WPP-V0, V-0 at 1.6 mm, for electrical housings, connectors, appliance parts, control boxes, flame-retardant structural parts and molded PP components. DEYU supports custom formulas, sample validation, bulk purchase and wholesale procurement.

Important parameters

Base resin
PP
Model
DGK-PP WPP-V0
Color
Custom color matching supported
Processing
Injection molding / extrusion. Injection molding, extrusion or other processes according to the formula.
Key performance
Halogen-free V-0 flame retardant; 1.6 mm can be tested to V-0; glow wire can be customized.
Status
Pellet compound

FAQ

Can this material be color matched?

Yes. DEYU can match black, natural, white or custom colors according to the base resin, filler system and target appearance.

Can flame retardancy be customized for a specific wall thickness?

Yes. The formula can be adjusted around UL94 level, wall thickness, color and impact requirement.

Can international orders receive certification documents?

Yes. DEYU can provide material data sheets and common export documents, and can coordinate RoHS, REACH, UL-related or other third-party testing according to the order requirement.

How can I get a sample of DGK-PP WPP-V0 or a similar material?

Submit the target resin, color, process and performance range. DEYU will suggest a sample grade or prepare a trial formula for sample validation. Request sample

Application areas

Application areaTypical parts
Application area 1electrical housings
Application area 2terminal blocks
Application area 3switch boxes
Application area 4charger shells
Application area 5wire harness clips
Application area 6control module covers

Reference quote

Minimum price
USD 5.9/kg
Maximum price
USD 10.8/kg
Delivery
Tax-included reference price; freight is not included.
Stock
Standard stock reference: 1000 kg. Special color, performance or certification requirements require custom production.

Final quotation depends on the specific formula, color, order volume and testing requirements.

Product Inquiry >

Data sheet

Physical Property Data Sheet

NamePP compositeSpecificationDGK-PP WPP-V0
Material propertiesHalogen-free eco flame-retardant, heat-resistant, high-impactColorNatural color
Use80 x 10 x 4 mmSample statePellets
Processing methodInjection molding-/
ItemConditionMethodDataUnit
Mechanical Properties
Bending strength/GB/T 9341-200835MPa
Flexural modulus/GB/T 9341-20081450MPa
Tensile strength20 mm/minGB/T 1040-200626MPa
Yield strength/GB/T 1040-200626MPa
Elongation at break/GB/T 1040-200630%
Charpy notched impact strength/GB/T 1043.1-200840J/m
Charpy unnotched impact strength/GB/T 1043.1-200845J/m
Izod notched impact strength/GB/T 1843-200060J/m
Others
Melt Flow Index/GB/T 3682-200010g/10 min
Density/GB/T 1033-19861.2g/cm3
Heat distortion temperatureMethod A, 120℃GB/T 1633-2000140℃
Surface resistivity/GB/T 1401-200210^15ohm/sq
FlammabilityUL-94GB/T 2408-1996V0/5VA/
Injection molding process
Drying temperature90℃Drying time4-5 h
Injection temperature190-210℃Mold temperature80℃

Contact