Conductive Extrusion PP Pellets DGK-PP DD3R1
Extrusion-grade conductive polypropylene with 10^3-10^5 ohm/sq surface resistivity
Conductive 10^3-10^5 ohm/sq, smooth glossy extrusion and no pitting.
DGK-PP DD3R1 is designed for conductive sheet and conductive filament extrusion. It balances stable conductivity, bright surface appearance and clean extrusion flow, making it suitable for ESD packaging, shielding fabric yarns, cable wrapping tapes and conductive spacer strips.
Important parameters
- Base resin
- PP
- Model
- DGK-PP DD3R1
- Color
- Black; custom black-tone matching supported
- Processing
- Extrusion / injection molding
- Key performance
- Conductive 10^3-10^5 ohm/sq; smooth glossy no-pitting extrusion surface.
- Status
- Pellet compound
FAQ
Can the surface resistivity be customized?
Yes. DEYU can adjust the formula around sheet thickness, filament diameter, grounding path and target resistance.
Can the extrusion surface be made brighter?
Yes. The grade is designed for glossy no-pitting extrusion, and the surface can be tuned with process and formula adjustments.
What applications is this grade mainly used for?
It is mainly used for conductive sheets, conductive filaments, ESD packaging filaments, shielding fabric yarns, cable wrapping tapes and conductive spacer strips.
How can I get a sample of DGK-PP DD3R1?
Send the target product size, extrusion process, resistance requirement and surface appearance requirement. DEYU will suggest a sample grade for validation. Request sample
Application areas
| Application area | Typical parts |
|---|---|
| Conductive sheet extrusion | ESD sheets, conductive divider sheets, anti-static packaging sheets |
| Conductive filament extrusion | Conductive monofilaments, brush filaments, shielding fabric yarns |
| ESD packaging | Conductive tying filaments, conductive packaging nets, anti-static support strips |
| Shielding textiles | Conductive yarns for shielding cloth, woven tape and grounding fabric |
| Electrical protection | Cable wrapping tapes, conductive spacer strips and separator strips |
| Custom extrusion parts | Glossy black profiles and thin strips requiring stable resistance |
Reference quote
- Minimum price
- USD 4.52/kg
- Maximum price
- USD 7.5/kg
- Delivery
- Tax-included reference price; freight is not included.
- Stock
- Standard stock reference: 1000 kg. Special color, surface finish, resistance range or certification requirements require custom production.
Final quotation depends on the specific formula, surface finish, color, order volume and testing requirements.
Data sheet
Physical Property Data Sheet
| Name | PP composite | Grade / Specification | DGK-PP DD3R1 |
|---|---|---|---|
| Material properties | Conductive extrusion-grade PP | Color | Black |
| Use | Conductive sheets, conductive filaments, ESD packaging, shielding fabric yarns | Sample state | Pellets |
| Processing method | Extrusion / injection molding | ||
| Item | Condition | Method | Data | Unit |
|---|---|---|---|---|
| Mechanical Properties | ||||
| Bending strength | - | GB/T 9341-2008 | 28.2 | MPa |
| Flexural modulus | - | GB/T 9341-2008 | 968.1 | MPa |
| Tensile strength | 50 mm/min | GB/T 1040-2006 | 21 | MPa |
| Elongation at break | 50 mm/min | GB/T 1040-2006 | 60 | % |
| Charpy notched impact strength | 23°C | GB/T 1043.1-2008 | 17.8 | kJ/m² |
| Charpy unnotched impact strength | 23°C | GB/T 1043.1-2008 | 99 | kJ/m² |
| Izod notched impact strength | 23°C | GB/T 1843-2000 | 19 | kJ/m² |
| Others | ||||
| Melt Flow Index | 230°C / 2.16 kg | GB/T 3682-2000 | 3.5 | g/10 min |
| Density | - | GB/T 1033-1986 | 1.046 | g/cm³ |
| Heat Distortion Temperature | 0.45 MPa | GB/T 1633-2000 | 81 | °C |
| Surface resistivity | - | GB/T 1401-2002 | 10³-10⁵ | ohm/sq |
| Flammability | UL-94 | GB/T 2408-1996 | HB | - |
| Shore hardness D | - | - | 73 | D |
| Injection molding process | ||||
| Drying temperature | 80°C | Drying time | 4-5 h | |
| Injection temperature | 200-230°C | Mold temperature | 50-70°C | |
Contact
Focused on modified plastic R&D and production
We provide professional customization services. If you have material questions, selection difficulties or performance requirements, contact us through any method on the right.
- Email: market@deyuplastics.com
- WeChat: mkx13905842100
- WhatsApp: +86 13905842100+86 15325909695
- Telegram: @deyuplast1