PTFE Wear-Resistant POM Pellets DGK-POM TF90M
POM with 20% PTFE for low-friction gears, sliders, bearings and guides
Contains 20% PTFE wear additive; low friction coefficient.
PTFE wear-resistant POM compound DGK-POM TF90M with 20% PTFE additive for gears, sliders, bearings, guide rails, low-friction assemblies and precision moving parts needing reduced wear. DEYU supports custom formulas, sample validation, bulk purchase and wholesale procurement.
Important parameters
- Base resin
- POM
- Model
- DGK-POM TF90M
- Color
- Custom color matching supported
- Processing
- Injection molding. Injection molding, extrusion or other processes according to the formula.
- Key performance
- Contains 20% PTFE wear additive; low friction coefficient.
- Status
- Pellet compound
FAQ
Can this material be color matched?
Yes. DEYU can match black, natural, white or custom colors according to the base resin, filler system and target appearance.
Can wear resistance and friction be customized?
Yes. PTFE, MoS2, aramid or other wear additives can be adjusted according to the mating material, load and movement speed.
Can international orders receive certification documents?
Yes. DEYU can provide material data sheets and common export documents, and can coordinate RoHS, REACH, UL-related or other third-party testing according to the order requirement.
How can I get a sample of DGK-POM TF90M or a similar material?
Submit the target resin, color, process and performance range. DEYU will suggest a sample grade or prepare a trial formula for sample validation. Request sample
Application areas
| Application area | Typical parts |
|---|---|
| Application area 1 | chair castors |
| Application area 2 | gears |
| Application area 3 | guide sliders |
| Application area 4 | bushings |
| Application area 5 | rollers |
| Application area 6 | textile machine sliding parts |
Reference quote
- Minimum price
- USD 5.9/kg
- Maximum price
- USD 10.8/kg
- Delivery
- Tax-included reference price; freight is not included.
- Stock
- Standard stock reference: 1000 kg. Special color, performance or certification requirements require custom production.
Final quotation depends on the specific formula, color, order volume and testing requirements.
Data sheet
Physical Property Data Sheet
| Name | POM/PTFE composite | Specification | DGK-POM TF90M |
|---|---|---|---|
| Material properties | Wear-resistant, self-lubricating | Color | Natural color |
| Use | Automotive parts, bushings, gear parts, etc. | Sample state | Pellets |
| Processing method | Injection molding | - | / |
| Item | Condition | Method | Data | Unit |
|---|---|---|---|---|
| Mechanical Properties | ||||
| Bending strength | 2 mm/min | GB/T 9341-2008 | 67 | MPa |
| Flexural modulus | 2 mm/min | GB/T 9341-2008 | 1742 | MPa |
| Tensile strength | 50 mm/min | GB/T 1040-2006 | 45 | MPa |
| Tensile modulus | 50 mm/min | GB/T 1040-2006 | 565 | MPa |
| Elongation at break | 50 mm/min | GB/T 1040-2006 | 35 | % |
| Charpy notched impact strength | 23℃ | GB/T 1043.1-2008 | 3.8 | kJ/m2 |
| Charpy unnotched impact strength | 23℃ | GB/T 1043.1-2008 | 49.5 | kJ/m2 |
| Izod notched impact strength | 23℃ | GB/T 1843-2000 | 8 | kJ/m2 |
| Others | ||||
| Melt Flow Index | 190℃ / 2.16 kg | GB/T 3682-2000 | 10.4 | g/10 min |
| Density | / | GB/T 1033-1986 | 1.53 | g/cm3 |
| Heat distortion temperature | 0.45 MPa | GB/T 1634-2000 | 123.8 | ℃ |
| Surface resistivity | / | GB/T 1401-2002 | 10^9 | ohm/sq |
| Flammability | UL-94 | GB/T 2408-1996 | HB | / |
| Injection molding process | ||||
| Drying temperature | 90℃ | Drying time | 4-5 h | |
| Injection temperature | 190-210℃ | Mold temperature | 80℃ | |
Contact
Focused on modified plastic R&D and production
We provide professional customization services. If you have material questions, selection difficulties or performance requirements, contact us through any method on the right.
- Email: market@deyuplastics.com
- WeChat: mkx13905842100
- WhatsApp: +86 13905842100+86 15325909695
- Telegram: @deyuplast1