Permanent Antistatic HDPE Pellets DGK-PE KJD789R1
Permanent antistatic HDPE with color-matching support
Natural-color HDPE with 10^7-10^9 ohm/sq antistatic performance for hollow parts, tubes, profiles, crates, trays and packaging components.
DGK-PE KJD789R1 is a permanent antistatic HDPE compound supplied in natural color and available for color matching. Its antistatic system is built into the HDPE matrix so charge can dissipate in the 10^7-10^9 ohm/sq range without relying on a temporary surface treatment. Injection molding, extrusion and blow molding can be evaluated for crates, trays, tubes, sleeves, profiles, hollow parts, packaging liners and logistics containers. Confirm final resistance on molded parts under the agreed test conditions.
Important parameters
- Base resin
- HDPE
- Model
- DGK-PE KJD789R1
- Product series
- Antistatic plastics
- Processing
- Injection molding, extrusion and blow molding
- Key performance
- Natural-color HDPE with 10^7-10^9 ohm/sq antistatic performance for hollow parts, tubes, profiles, crates, trays and packaging components.
- Main application
- Antistatic hollow parts
- Customization
- Natural color; color matching available
FAQ
What makes this PE permanently antistatic?
Its antistatic system is built into the HDPE matrix rather than applied as a temporary surface coating. Finished-part testing remains necessary.
Can the color be matched?
Yes. Natural-color material can be color matched; confirm resistance and appearance on the color-matched molded lot.
Which processes are applicable?
Injection molding, extrusion and blow molding can be evaluated for the target part, machine and dimensions.
How should resistance be verified?
Test the finished part under the agreed humidity, probe arrangement, wall thickness and surface condition, not pellets alone.
Application Areas
| Main application | Project quotation |
|---|---|
| Antistatic hollow parts | Blow-molded floats, filter balls and hollow parts requiring charge dissipation. |
| Tubes and profiles | Extruded antistatic tubes, sleeves and profiles for powder, liquid and wire protection. |
| Electronics handling | Crates, trays, liners and housings for ESD-controlled handling areas. |
| Packaging and logistics | Antistatic dividers, boxes and returnable containers with color-matching support. |
Quote
Contact DEYU for pricing and sample availability based on the grade, quantity, color and validation requirements.
Product Inquiry >Data sheet
Physical Property Data Sheet
| Model | DGK-PE KJD789R1 | Base resin | HDPE |
|---|---|---|---|
| Product series | Antistatic plastics | Customization | Natural color; color matching available |
| Processing | Injection molding, extrusion and blow molding | Sample support | Pellets |
| Item | Condition | Method | Data | Unit |
|---|---|---|---|---|
| Electrical properties | ||||
| Surface resistivity | Typical value | GB/T 1401-2002 | 10^7-10^9 | ohm/sq |
| Basic properties | ||||
| Melt flow rate | Typical value | GB/T 3682-2000 | 9.6 | g/10 min |
| Density | Typical value | GB/T 1033-1986 | 0.98 | g/cm3 |
| Mechanical properties | ||||
| Flexural strength | 2 mm/min | GB/T 9341-2008 | 27 | MPa |
| Flexural modulus | 2 mm/min | GB/T 9341-2008 | 1260 | MPa |
| Tensile strength | 50 mm/min | GB/T 1040-2006 | 18 | MPa |
| Yield strength | 50 mm/min | GB/T 1040-2006 | 17.2 | MPa |
| Elongation at break | 50 mm/min | GB/T 1040-2006 | 30.8 | % |
| Charpy notched impact strength | 23 C | GB/T 1043.1-2008 | 15 | kJ/m2 |
| Charpy unnotched impact strength | 23 C | GB/T 1043.1-2008 | No break | kJ/m2 |
| Izod notched impact strength | 23 C | GB/T 1843-2000 | 19.2 | kJ/m2 |
| Thermal properties | ||||
| Heat distortion temperature | Method A | GB/T 1633-2000 | 93 | C |
| Flammability | 1.6 mm | GB/T 2408-1996 | HB | / |
Reference: dry at 85 C for 4-5 h; injection 195-210 C; mold 70 C. Confirm extrusion and blow-molding settings by part trial.
Values are reproduced from the Chinese product source. Confirm the electrical quantity, units, original test-method identifier and thermal-property designation against the signed report before acceptance; a material value is not a finished-part certification.
Contact
Focused on modified plastic R&D and production
We provide professional customization services. If you have material questions, selection difficulties or performance requirements, contact us through any method on the right.
- Email: market@deyuplastics.com
- WeChat: mkx13905842100
- WhatsApp: +86 13905842100+86 15325909695