Conductive PE Pellets DGK-PE DD4JC

Conductive PE that retains polyethylene flexibility and low-temperature toughness

A 10^3-10^4 ohm/sq conductive PE for gas-pipeline coating and jacketing, extrusion profiles and flexible industrial parts.

DGK-PE DD4JC is a black conductive PE compound developed for applications that need flexibility, impact resistance and conductivity together. The material keeps PE elongation and chemical stability while reaching 10^3-10^4 ohm/sq surface resistivity. It is suited to extruded coating, jacketing, sheet and profile, as well as selected injection-molded parts. For gas-pipeline coating or corrugated protective pipe, use it only after confirming pipe construction, cathodic-protection system, grounding, environmental exposure and the governing project specification.

Important parameters

Base resin
PE
Model
DGK-PE DD4JC
Product series
Conductive plastics
Processing
Extrusion and injection molding
Key performance
A 10^3-10^4 ohm/sq conductive PE for gas-pipeline coating and jacketing, extrusion profiles and flexible industrial parts.
Main application
Gas-pipeline coating and jacketing
Customization
Black

FAQ

Why is high elongation important for corrugated pipe or coating?

Flexible coating and corrugated protection must follow pipe movement, settlement and installation bending. Confirm the required deformation on the actual construction.

Does a conductive PE alone complete the safety system?

No. Static control also depends on construction, bonding, grounding, cathodic protection, installation and the governing project standard.

Can DD4JC be extruded?

Yes, it is an extrusion and injection-molding direction. Set melt temperature, die pressure, line speed and cooling through an actual coating or profile trial.

How should resistance be accepted?

Verify finished parts to the agreed method, position, conditioning and acceptance range; do not use pellet readings as final part acceptance.

Application Areas

Main applicationProject quotation
Gas-pipeline coating and jacketingConductive PE coating or protective jacketing subject to project-specific verification.
Corrugated protective pipeFlexible protective pipe or sleeve where resistance, construction and grounding are confirmed together.
Repair patches and wrapPatch, wrap and heat-shrink tape base-material directions requiring process consistency.
Extruded sheet and profilesConductive PE sheet, profile and jacketing applications needing flexible service.

Quote

Contact DEYU for pricing and sample availability based on the grade, quantity, color and validation requirements.

Product Inquiry >
Product Inquiry >

Data sheet

Physical Property Data Sheet

ModelDGK-PE DD4JCBase resinPE
Product seriesConductive plasticsCustomizationBlack
ProcessingExtrusion and injection moldingSample supportPellets
ItemConditionMethodDataUnit
Electrical properties
Surface resistivityTypical valueGB/T 1401-200210^3-10^4ohm/sq
Basic properties
Melt flow rateTypical valueGB/T 3682-20003.2g/10 min
DensityTypical valueGB/T 1033-19860.91g/cm3
Mechanical properties
Flexural strength2 mm/minGB/T 9341-20087.46MPa
Flexural modulus2 mm/minGB/T 9341-2008361MPa
Tensile strength20 mm/minGB/T 1040-200618MPa
Yield strength20 mm/minGB/T 1040-20068.7MPa
Elongation at break20 mm/minGB/T 1040-2006538%
Charpy notched impact strengthTypical valueGB/T 1043.1-200835kJ/m2
Charpy unnotched impact strengthTypical valueGB/T 1043.1-2008No breakkJ/m2
Thermal properties
Heat distortion temperatureMethod AGB/T 1633-200095C
FlammabilityUL 94GB/T 2408-1996HB/

Reference: dry at 90 C for 3-4 h; injection 225-230 C; mold 80 C. Confirm extrusion settings on the coating or profile line.

Values are reproduced from the Chinese product source. Confirm the electrical quantity, units, original test-method identifier and thermal-property designation against the signed report before acceptance; a material value is not a finished-part certification.