Flame-Retardant PC Pellets DGK-PC FR3000
V-0 flame-retardant PC for electrical, electronic and engineering molded parts
Flame-retardant PC; V-0 grade; titanium-white sample with custom color matching support.
Flame-retardant PC compound DGK-PC FR3000, V-0 grade, for electrical housings, electronic accessories, automotive parts, appliance components, control covers and molded parts requiring flame resistance. DEYU supports custom formulas, sample validation, bulk purchase and wholesale procurement.
Important parameters
- Base resin
- PC
- Model
- DGK-PC FR3000
- Color
- Custom color matching supported
- Processing
- Injection molding. Injection molding, extrusion or other processes according to the formula.
- Key performance
- Flame-retardant PC; V-0 grade; titanium-white sample with custom color matching support.
- Status
- Pellet compound
FAQ
Can this material be color matched?
Yes. DEYU can match black, natural, white or custom colors according to the base resin, filler system and target appearance.
Can flame retardancy be customized for a specific wall thickness?
Yes. The formula can be adjusted around UL94 level, wall thickness, color and impact requirement.
Can international orders receive certification documents?
Yes. DEYU can provide material data sheets and common export documents, and can coordinate RoHS, REACH, UL-related or other third-party testing according to the order requirement.
How can I get a sample of DGK-PC FR3000 or a similar material?
Submit the target resin, color, process and performance range. DEYU will suggest a sample grade or prepare a trial formula for sample validation. Request sample
Application areas
| Application area | Typical parts |
|---|---|
| Application area 1 | electrical housings |
| Application area 2 | terminal blocks |
| Application area 3 | switch boxes |
| Application area 4 | charger shells |
| Application area 5 | wire harness clips |
| Application area 6 | control module covers |
Reference quote
- Minimum price
- USD 5.9/kg
- Maximum price
- USD 10.8/kg
- Delivery
- Tax-included reference price; freight is not included.
- Stock
- Standard stock reference: 1000 kg. Special color, performance or certification requirements require custom production.
Final quotation depends on the specific formula, color, order volume and testing requirements.
Data sheet
Physical Property Data Sheet
| Name | PC composite | Specification | DGK-PC FR3000 |
|---|---|---|---|
| Material properties | Flame-retardant | Color | Titanium white |
| Use | Automotive parts, electronic accessories, etc. | Sample state | Pellets |
| Processing method | Injection molding | - | / |
| Item | Condition | Method | Data | Unit |
|---|---|---|---|---|
| Mechanical Properties | ||||
| Bending strength | / | GB/T 9341-2008 | 89 | MPa |
| Flexural modulus | / | GB/T 9341-2008 | 3015 | MPa |
| Tensile strength | 20 mm/min | GB/T 1040-2006 | 65.8 | MPa |
| Yield strength | / | GB/T 1040-2006 | 65.7 | MPa |
| Elongation at break | / | GB/T 1040-2006 | 75 | % |
| Charpy notched impact strength | / | GB/T 1043.1-2008 | 16 | kJ/m2 |
| Charpy unnotched impact strength | / | GB/T 1043.1-2008 | No fracture | kJ/m2 |
| Izod notched impact strength | / | GB/T 1843-2000 | 26.8 | kJ/m2 |
| Others | ||||
| Melt Flow Index | / | GB/T 3682-2000 | 16 | g/10 min |
| Density | / | GB/T 1033-1986 | 1.26 | g/cm3 |
| Heat distortion temperature | Method A, 120℃ | GB/T 1633-2000 | 112 | ℃ |
| Surface resistivity | / | GB/T 1401-2002 | 10^16 | ohm/sq |
| Flammability | UL-94 | GB/T 2408-1996 | V0 | / |
| Injection molding process | ||||
| Drying temperature | 105℃ | Drying time | 4-5 h | |
| Injection temperature | 255-270℃ | Mold temperature | 80℃ | |
Contact
Focused on modified plastic R&D and production
We provide professional customization services. If you have material questions, selection difficulties or performance requirements, contact us through any method on the right.
- Email: market@deyuplastics.com
- WeChat: mkx13905842100
- WhatsApp: +86 13905842100+86 15325909695
- Telegram: @deyuplast1