Wood Fiber PA6 Composite Pellets DGK-PA6 PA28 335M

Bio-based PA6 compound with wood-fiber texture, high hardness and wear resistance

Bio-based PA6 compound with wood-fiber texture, high hardness, heat resistance, wear resistance and slight wood aroma.

Wood fiber PA6 composite DGK-PA6 PA28 335M with high hardness, heat resistance, wear resistance and wood-like texture for bio-based molded parts, pet products, durable consumer goods and structural appearance parts. DEYU supports custom formulas, sample validation, bulk purchase and wholesale procurement.

Important parameters

Base resin
PA6
Model
DGK-PA6 PA28 335M
Color
Custom color matching supported
Processing
Injection molding. Injection molding, extrusion or other processes according to the formula.
Key performance
Bio-based PA6 compound with wood-fiber texture, high hardness, heat resistance, wear resistance and slight wood aroma.
Status
Pellet compound

FAQ

Can this material be color matched?

Yes. DEYU can match black, natural, white or custom colors according to the base resin, filler system and target appearance.

Can wear resistance and friction be customized?

Yes. PTFE, MoS2, aramid or other wear additives can be adjusted according to the mating material, load and movement speed.

Can international orders receive certification documents?

Yes. DEYU can provide material data sheets and common export documents, and can coordinate RoHS, REACH, UL-related or other third-party testing according to the order requirement.

How can I get a sample of DGK-PA6 PA28 335M or a similar material?

Submit the target resin, color, process and performance range. DEYU will suggest a sample grade or prepare a trial formula for sample validation. Request sample

Application areas

Application areaTypical parts
Application area 1chair castors
Application area 2gears
Application area 3guide sliders
Application area 4bushings
Application area 5rollers
Application area 6textile machine sliding parts

Reference quote

Minimum price
USD 5.9/kg
Maximum price
USD 10.8/kg
Delivery
Tax-included reference price; freight is not included.
Stock
Standard stock reference: 1000 kg. Special color, performance or certification requirements require custom production.

Final quotation depends on the specific formula, color, order volume and testing requirements.

Product Inquiry >

Data sheet

Physical Property Data Sheet

NameDGK-PA6 PA28 335MSpecificationDGK-PA6 PA28 335M
Material propertiesEnvironment-friendly, high hardness, heat-resistant, wear-resistantColorBeige
UseBio-based injection molded componentsSample statePellets
Processing methodInjection molding-/
ItemConditionMethodDataUnit
Basic Properties
Density/ASTM D-7921.35g/cm3
Melt Flow Index///g/10 min
Mechanical Properties
Tensile strength50 mm/minASTM D-63843MPa
Elongation at break50 mm/minASTM D-6385%
Bending strength10 mm/minASTM D-79074MPa
Flexural modulus10 mm/minASTM D-7904080MPa
Izod notched impact strength23℃ASTM D-2565.8kJ/m2
Izod unnotched impact strength23℃ASTM D-25675HD
Electrical Properties
Surface resistivity/ASTM D-25710^9ohm/sq
Thermal Properties
Melting point/ASTM D-789205℃
Others
Limited oxygen index///%
FlammabilityUL-94/HB/
Injection molding process
Drying temperature110-130℃Drying time4-5 h
Injection temperature195-235℃Mold temperature80-90℃