Conductive HDPE Pellets DGK-HDPE DD4-5CS

Conductive HDPE for blow molded and injection molded transport drums

Surface resistivity around 10^4-10^5 ohm/sq, chemical resistance and impact performance for drum bodies, lids, flanges and fittings.

DGK-HDPE DD4-5CS is a black conductive HDPE compound for thick-wall hollow parts. Its carbon-black conductive network gives drums, canisters and tanks a path for charge dissipation while retaining HDPE chemical resistance, moisture resistance and handling toughness. Typical references include precious-metal powder drums, explosion-proof drums, chemical transport drums, conductive liners and hoppers. The finished drum must be tested and bonded to the site grounding arrangement where the application requires it.

Important parameters

Base resin
HDPE
Model
DGK-HDPE DD4-5CS
Product series
Conductive plastics
Processing
Blow molding and injection molding
Key performance
Surface resistivity around 10^4-10^5 ohm/sq, chemical resistance and impact performance for drum bodies, lids, flanges and fittings.
Main application
Precious-metal powder drums
Customization
Black

FAQ

Why use conductive HDPE for transport drums?

A conductive wall provides a route for static-charge dissipation while HDPE supplies chemical resistance and impact performance for thick-wall containers.

Can it be blow molded and injection molded?

Yes. Drum bodies, canisters and tanks are typical blow-molding directions; lids, flanges, handles and sealing parts can be evaluated by injection molding.

What must be confirmed for flammable service?

Confirm the resistance target, drum geometry, filled weight, drop test, grounding point and site safety procedure on the finished container.

Which processing data are reference only?

Drying, melt, parison, die and cooling settings are machine and drum dependent. Validate them in a trial rather than transferring pellet data directly.

Application Areas

Main applicationProject quotation
Precious-metal powder drumsConductive blow-molded drums that limit static accumulation and powder adhesion.
Explosion-proof drumsDrum bodies that can be bonded and earthed within the site's safety procedure.
Chemical transport drumsHDPE transport drums for acids, alkalis and solvents requiring impact performance.
Lids and fittingsInjection-molded lids, flanges, handles and sealing components for conductive containers.

Quote

Contact DEYU for pricing and sample availability based on the grade, quantity, color and validation requirements.

Product Inquiry >
Product Inquiry >

Data sheet

Physical Property Data Sheet

ModelDGK-HDPE DD4-5CSBase resinHDPE
Product seriesConductive plasticsCustomizationBlack
ProcessingBlow molding and injection moldingSample supportPellets
ItemConditionMethodDataUnit
Electrical properties
Surface resistivityTypical valueGB/T 1401-200210^4-10^5ohm/sq
Basic properties
Melt flow rate190 C / 2.16 kgGB/T 36820.336g/10 min
Melt flow rate190 C / 5 kgGB/T 36822.34g/10 min
DensityTypical valueGB/T 10331.053g/cm3
Mechanical properties
Tensile strength50 mm/minGB/T 104020.676MPa
Tensile modulus50 mm/minGB/T 1040280.377MPa
Elongation at break50 mm/minGB/T 1040139.459%
Flexural strength2 mm/minGB/T 934120.006MPa
Flexural modulus2 mm/minGB/T 9341614.65MPa
Izod notched impact strength23 CGB/T 184315.7kJ/m2
Izod unnotched impact strength23 CGB/T 1843108.1kJ/m2
Charpy notched impact strength23 CGB/T 104315.1kJ/m2
Charpy unnotched impact strength23 CGB/T 104392.4kJ/m2
Thermal properties
Heat distortion temperature0.45 MPaGB/T 163466.4C

Drying reference: 100 C for 180 min. Set melt, parison and cooling by the actual drum design.

Values are reproduced from the Chinese product source. Confirm the electrical quantity, units, original test-method identifier and thermal-property designation against the signed report before acceptance; a material value is not a finished-part certification.