Low-Temperature Resistant ABS Pellets DGK-ABS NDW140U
Low-temperature resistant ABS for cold-use housings, liners and molded parts
Natural ABS with low-temperature and weather resistance; tensile strength 45 MPa, bending strength 64 MPa, tensile modulus 3600 MPa and HB flammability.
Low-temperature resistant ABS compound DGK-ABS NDW140U for refrigerator liners, door panels, cold-use appliance parts, outdoor housings, storage components and molded parts requiring toughness in low-temperature environments. DEYU supports custom formulas, sample validation, bulk purchase and wholesale procurement.
Important parameters
- Base resin
- ABS
- Model
- DGK-ABS NDW140U
- Color
- Custom color matching supported
- Processing
- Injection molding. Injection molding, extrusion or other processes according to the formula.
- Key performance
- Natural ABS with low-temperature and weather resistance; tensile strength 45 MPa, bending strength 64 MPa, tensile modulus 3600 MPa and HB flammability.
- Status
- Pellet compound
FAQ
Can this material be color matched?
Yes. DEYU can match black, natural, white or custom colors according to the base resin, filler system and target appearance.
Can flame retardancy be customized for a specific wall thickness?
Yes. The formula can be adjusted around UL94 level, wall thickness, color and impact requirement.
Can international orders receive certification documents?
Yes. DEYU can provide material data sheets and common export documents, and can coordinate RoHS, REACH, UL-related or other third-party testing according to the order requirement.
How can I get a sample of DGK-ABS NDW140U or a similar material?
Submit the target resin, color, process and performance range. DEYU will suggest a sample grade or prepare a trial formula for sample validation. Request sample
Application areas
| Application area | Typical parts |
|---|---|
| Application area 1 | electrical housings |
| Application area 2 | terminal blocks |
| Application area 3 | switch boxes |
| Application area 4 | charger shells |
| Application area 5 | wire harness clips |
| Application area 6 | control module covers |
Reference quote
- Minimum price
- USD 5.9/kg
- Maximum price
- USD 10.8/kg
- Delivery
- Tax-included reference price; freight is not included.
- Stock
- Standard stock reference: 1000 kg. Special color, performance or certification requirements require custom production.
Final quotation depends on the specific formula, color, order volume and testing requirements.
Data sheet
Physical Property Data Sheet
| Name | ABS composite | Specification | DGK-ABS NDW140U |
|---|---|---|---|
| Material properties | Low-temperature resistant, weather-resistant | Color | Natural |
| Use | Refrigerator liner, refrigerator door panel, etc. | Sample state | Pellets |
| Processing method | Injection molding | - | / |
| Item | Condition | Method | Data | Unit |
|---|---|---|---|---|
| Mechanical Properties | ||||
| Bending strength | / | ASTM D-790 | 64 | MPa |
| Modulus of elasticity | / | ASTM D-790 | / | MPa |
| Tensile modulus | / | ASTM D-638 | 3600 | MPa |
| Elongation at break | / | ASTM D-638 | 20 | % |
| Tensile strength | / | ASTM D-638 | 45 | MPa |
| Others | ||||
| Density | 23℃ | ASTM D-792 | 1.04 | g/cm3 |
| Forming shrinkage | / | ASTM D-955 | 0.4-0.7 | % |
| Melt Flow Index | 220℃ / 5 kg | ASTM D-1238 | 2.9 | g/10 min |
| Heat distortion temperature | 18.6 kg/cm2, unannealed | ASTM D-648 | 85 | ℃ |
| Rockwell hardness | / | ASTM D-785 | 100 | R |
| Vicat softening point | / | ASTM D-1525 | 95 | ℃ |
| Flammability | / | UL-94 | HB | / |
| Injection molding process | ||||
| Drying temperature | 90℃ | Drying time | 4-5 h | |
| Injection temperature | 210-225℃ | Mold temperature | 80℃ | |
Contact
Focused on modified plastic R&D and production
We provide professional customization services. If you have material questions, selection difficulties or performance requirements, contact us through any method on the right.
- Email: market@deyuplastics.com
- WeChat: mkx13905842100
- WhatsApp: +86 13905842100+86 15325909695
- Telegram: @deyuplast1