Transparent Antistatic ABS Pellets DGK-ABS KJD890TM
Transparent permanent antistatic ABS with 10^8-10^10 ohm/sq resistance
Permanent transparent antistatic ABS; surface resistivity 10^8-10^10 ohm/sq; light transmittance above 85%.
Transparent antistatic ABS compound DGK-ABS KJD890TM with 10^8-10^10 ohm/sq resistance for clear ESD covers, observation windows, transparent guards, electronic panels and visible antistatic molded parts. DEYU supports custom formulas, sample validation, bulk purchase and wholesale procurement.
Important parameters
- Base resin
- ABS
- Model
- DGK-ABS KJD890TM
- Color
- Custom color matching supported
- Processing
- Injection molding / extrusion. Injection molding, extrusion or other processes according to the formula.
- Key performance
- Permanent transparent antistatic ABS; surface resistivity 10^8-10^10 ohm/sq; light transmittance above 85%.
- Status
- Pellet compound
FAQ
Can this material be color matched?
Yes. DEYU can match black, natural, white or custom colors according to the base resin, filler system and target appearance.
Can the resistance or ESD level be customized?
Yes. Resistance range, stiffness and processing balance can be adjusted according to wall thickness, part design and grounding requirements.
Can international orders receive certification documents?
Yes. DEYU can provide material data sheets and common export documents, and can coordinate RoHS, REACH, UL-related or other third-party testing according to the order requirement.
How can I get a sample of DGK-ABS KJD890TM or a similar material?
Submit the target resin, color, process and performance range. DEYU will suggest a sample grade or prepare a trial formula for sample validation. Request sample
Application areas
| Application area | Typical parts |
|---|---|
| Application area 1 | Transparent ESD covers |
| Application area 2 | Observation windows |
| Application area 3 | Transparent equipment guards |
| Application area 4 | Electronic display panels |
| Application area 5 | Visible antistatic molded parts |
| Application area 6 | Transparent antistatic molded parts |
Reference quote
- Minimum price
- USD 4.1/kg
- Maximum price
- USD 10.3/kg
- Delivery
- Tax-included reference price; freight is not included.
- Stock
- Standard stock reference: 1000 kg. Special color, performance or certification requirements require custom production.
Final quotation depends on the specific formula, color, order volume and testing requirements.
Data sheet
Physical Property Data Sheet
| Name | ABS composite | Specification | DGK-ABS KJD890TM |
|---|---|---|---|
| Material properties | Ultra-transparent, permanent anti-static | Color | High transparency |
| Use | 80 x 10 x 4 mm | Sample state | Pellets |
| Processing method | Injection molding | - | / |
| Item | Condition | Method | Data | Unit |
|---|---|---|---|---|
| Mechanical Properties | ||||
| Bending strength | 2 mm/min | GB/T 9341-2008 | 47 | MPa |
| Flexural modulus | 2 mm/min | GB/T 9341-2008 | 1375 | MPa |
| Tensile strength | 50 mm/min | GB/T 1040-2006 | 35.1 | MPa |
| Tensile modulus | 50 mm/min | GB/T 1040-2006 | 575 | MPa |
| Elongation at break | 50 mm/min | GB/T 1040-2006 | 40.5 | % |
| Charpy notched impact strength | 23℃ | GB/T 1043.1-2008 | 12.7 | kJ/m2 |
| Charpy unnotched impact strength | 23℃ | GB/T 1043.1-2008 | 99.4 | kJ/m2 |
| Izod notched impact strength | 23℃ | GB/T 1843-2000 | 15.3 | kJ/m2 |
| Others | ||||
| Melt Flow Index | 220℃ / 10 kg | GB/T 3682-2000 | 54.6 | g/10 min |
| Density | / | GB/T 1033-1986 | 1.115 | g/cm3 |
| Heat distortion temperature | 0.45 MPa | GB/T 1633-2000 | 84.5 | ℃ |
| Surface resistivity | / | GB/T 1401-2002 | 10^8-10^10 | ohm/sq |
| Flammability | UL-94 | GB/T 2408-1996 | HB | / |
| Injection molding process | ||||
| Drying temperature | 85℃ | Drying time | 4-5 h | |
| Injection temperature | 195-210℃ | Mold temperature | 70℃ | |
Contact
Focused on modified plastic R&D and production
We provide professional customization services. If you have material questions, selection difficulties or performance requirements, contact us through any method on the right.
- Email: market@deyuplastics.com
- WeChat: mkx13905842100
- WhatsApp: +86 13905842100+86 15325909695
- Telegram: @deyuplast1