Graphite Conductive ABS Pellets DGK-ABS DD3C

Graphite filled conductive ABS with 10^3-10^4 ohm/sq surface resistivity

Graphite composite conductive ABS; surface resistivity around 10^3-10^4 ohm/sq with antistatic and conductive performance.

Graphite conductive ABS compound DGK-ABS DD3C with 10^3-10^4 ohm/sq surface resistivity for ESD housings, electronic parts, disk-drive components, office equipment, antistatic molded parts and low-resistance applications. DEYU supports custom formulas, sample validation, bulk purchase and wholesale procurement.

Important parameters

Base resin
ABS
Model
DGK-ABS DD3C
Color
Custom color matching supported
Processing
Injection molding. Injection molding, extrusion or other processes according to the formula.
Key performance
Graphite composite conductive ABS; surface resistivity around 10^3-10^4 ohm/sq with antistatic and conductive performance.
Status
Pellet compound

FAQ

Can this material be color matched?

Yes. DEYU can match black, natural, white or custom colors according to the base resin, filler system and target appearance.

Can the resistance or ESD level be customized?

Yes. Resistance range, stiffness and processing balance can be adjusted according to wall thickness, part design and grounding requirements.

Can international orders receive certification documents?

Yes. DEYU can provide material data sheets and common export documents, and can coordinate RoHS, REACH, UL-related or other third-party testing according to the order requirement.

How can I get a sample of DGK-ABS DD3C or a similar material?

Submit the target resin, color, process and performance range. DEYU will suggest a sample grade or prepare a trial formula for sample validation. Request sample

Application areas

Application areaTypical parts
Application area 1ESD trays
Application area 2sensor housings
Application area 3medical device accessories
Application area 4conductive textile parts
Application area 5shielding covers
Application area 6low-resistance molded clips

Reference quote

Minimum price
USD 4.1/kg
Maximum price
USD 10.3/kg
Delivery
Tax-included reference price; freight is not included.
Stock
Standard stock reference: 1000 kg. Special color, performance or certification requirements require custom production.

Final quotation depends on the specific formula, color, order volume and testing requirements.

Product Inquiry >

Data sheet

Physical Property Data Sheet

NameABS compositeSpecificationDGK-ABS DD3C
Material propertiesConductive, anti-staticColorBlack
UseFloppy disk, fax machine and videotape housingsSample statePellets
Processing methodInjection molding-/
ItemConditionMethodDataUnit
Mechanical Properties
Bending strength/GB/T 9341-200834MPa
Flexural modulus/GB/T 9341-20081600MPa
Tensile strength20 mm/minGB/T 1040-200619MPa
Elongation at break/GB/T 1040-200617%
Izod notched impact strength/GB/T 1843-20008kJ/m2
Others
Melt Flow Index/GB/T 3682-20006g/10 min
Heat distortion temperatureMethod B, 120℃GB/T 1633-200084℃
Surface resistivity23℃GB/T 1401-200210^3-10^4ohm/sq
FlammabilityUL-94GB/T 2408-1996HB/
Injection molding process
Drying temperature90℃Drying time3-4 h
Injection temperature225-235℃Mold temperature/

Contact

Focused on modified plastic R&D and production

We provide professional customization services. If you have material questions, selection difficulties or performance requirements, contact us through any method on the right.