Carbon Fiber Reinforced ABS Pellets DGK-ABS CF15L
Carbon fiber ABS with >=138 MPa bending strength for conductive structural molding
Carbon fiber reinforced ABS; bending strength >=138 MPa; surface resistivity <=10^4 ohm-cm.
Carbon fiber reinforced ABS compound DGK-ABS CF15L with >=138 MPa bending strength and conductive behavior for housings, brackets, fixtures, ESD structural parts and high-strength molded components. Pellet supply and quote by volume. DEYU supports custom formulas, sample validation, bulk purchase and wholesale procurement.
Important parameters
- Base resin
- ABS
- Model
- DGK-ABS CF15L
- Color
- Custom color matching supported
- Processing
- Injection molding. Injection molding, extrusion or other processes according to the formula.
- Key performance
- Carbon fiber reinforced ABS; bending strength >=138 MPa; surface resistivity <=10^4 ohm-cm.
- Status
- Pellet compound
FAQ
Can this material be color matched?
Yes. DEYU can match black, natural, white or custom colors according to the base resin, filler system and target appearance.
Can stiffness and carbon fiber content be customized?
Yes. Fiber level, flow and shrinkage can be tuned around stiffness, part size and surface requirements.
Can international orders receive certification documents?
Yes. DEYU can provide material data sheets and common export documents, and can coordinate RoHS, REACH, UL-related or other third-party testing according to the order requirement.
How can I get a sample of DGK-ABS CF15L or a similar material?
Submit the target resin, color, process and performance range. DEYU will suggest a sample grade or prepare a trial formula for sample validation. Request sample
Application areas
| Application area | Typical parts |
|---|---|
| Application area 1 | lightweight brackets |
| Application area 2 | structural housings |
| Application area 3 | robot arm covers |
| Application area 4 | battery component holders |
| Application area 5 | precision frames |
| Application area 6 | metal-replacement supports |
Reference quote
- Minimum price
- USD 3.5/kg
- Maximum price
- USD 12.5/kg
- Delivery
- Tax-included reference price; freight is not included.
- Stock
- Standard stock reference: 1000 kg. Special color, performance or certification requirements require custom production.
Final quotation depends on the specific formula, color, order volume and testing requirements.
Data sheet
Physical Property Data Sheet
| Name | ABS composite | Specification | DGK-ABS CF15L |
|---|---|---|---|
| Material properties | High strength, carbon fiber composite | Color | Black |
| Use | 80 x 10 x 4 mm | Sample state | Pellets |
| Processing method | Injection molding | - | / |
| Item | Condition | Method | Data | Unit |
|---|---|---|---|---|
| Mechanical Properties | ||||
| Bending strength | 2 mm/min | GB/T 9341-2008 | >=138 | MPa |
| Flexural modulus | 2 mm/min | GB/T 9341-2008 | >=8160 | MPa |
| Tensile strength | 50 mm/min | GB/T 1040-2006 | >=97.6 | MPa |
| Tensile modulus | 50 mm/min | GB/T 3398.2-2008 | >=1926 | MPa |
| Elongation at break | 50 mm/min | GB/T 1040-2006 | >=5.5 | % |
| Charpy notched impact strength | 23℃ | GB/T 1043.1-2008 | >=6 | kJ/m2 |
| Charpy unnotched impact strength | 23℃ | GB/T 1043.1-2008 | >=10 | kJ/m2 |
| Izod unnotched impact strength | 23℃ | GB/T 1843-2000 | >=23 | kJ/m2 |
| Others | ||||
| Melt Flow Index | 230℃ / 10 kg | GB/T 3682-2000 | <=18 | g/10 min |
| Density | / | GB/T 1033-1986 | 1.096-1.1 | g/cm3 |
| Heat distortion temperature | 1.8 MPa | GB/T 1633-2000 | >=92 | ℃ |
| Surface resistivity | / | GB/T 1401-2002 | <=10^4 | ohm/sq |
| Flammability | UL-94 | GB/T 2408-1996 | HB | / |
Contact
Focused on modified plastic R&D and production
We provide professional customization services. If you have material questions, selection difficulties or performance requirements, contact us through any method on the right.
- Email: market@deyuplastics.com
- WeChat: mkx13905842100
- WhatsApp: +86 13905842100+86 15325909695
- Telegram: @deyuplast1