High-conductivity PP, conductivity >25 S/cm, for bipolar plates and conductive structural parts.
Conductive modification using carbon black, carbon fiber, graphite, carbon nanotube or compound conductive systems to adjust electrical resistance and mechanical balance.
Product Inquiry >DGK-PE300; DGK-PA20; DGK-POM10; DGK-ABS conductive series
Conductive modification using carbon black, carbon fiber, graphite, carbon nanotube or compound conductive systems to adjust electrical resistance and mechanical balance.
Injection molding / extrusion / compounding / pelletizing
Resistance range, base resin, color, strength, flowability and processing method.